Technical Data Sheet<br />

Thoroughly wash down/clean tropical woods and high-resin, tacky<br />

wooden surfaces using <strong>Tex</strong>-<strong>Color</strong> Nitroverdünnung and allow to flash<br />

off thoroughly. Pitch pockets must be burnt out. Corners must be<br />

rounded.<br />

The moisture content of the wood should be measured in several<br />

places at a depth of at least 5 mm. For softwood this should be no<br />

more than 15%, for hardwood no more than 12%.<br />

Greyed wood must be removed completely using mechanical<br />

techniques to reveal the healthy wood. Check that the substrate/old<br />

coating is suitably compatible with the new varnish before<br />

application.<br />

Also give consideration to the structural preservation of wood used<br />

outdoors. Damage to the coating may occur if the wood has not been<br />

structurally preserved properly.<br />

See also VOB*, Part C, DIN 18 363, Section 3, “Painters and<br />

varnishers” (*Contract procedures for building works - Part C;<br />

General technical specifications for building works).<br />

Application Guide<br />

<strong>Tex</strong>-<strong>Color</strong> Imprägnier-<strong>Lasur</strong> <strong>TC</strong> <strong>6303</strong> should be shaken or stirred<br />

before use, and occasionally whilst working.<br />

It is advisable to apply the product using artist's or decorator's<br />

brushes or by using a dipping method.<br />

Softwoods and hardwoods that are at risk from rot, fungus or blue<br />

stain must be impregnated with 2 coats of <strong>Tex</strong>-<strong>Color</strong> Holzschutzgrund<br />

<strong>TC</strong> 6301 farblos (colourless) by either brushing or dipping.<br />

Structural components and/or woods that are exposed to very harsh<br />

weathering effects should be provided with a further final coat of <strong>Tex</strong>-<br />

<strong>Color</strong> Imprägnier-<strong>Lasur</strong> <strong>TC</strong> <strong>6303</strong>. Please take into consideration that<br />

the colour of the finish will be intensified with each additional coat.<br />

Use Imprägnier-<strong>Lasur</strong> farblos (colourless) if required.<br />

Restorative work<br />

(After 2 - 3 years) Brush off surface and clean, apply one coat of<br />

<strong>Tex</strong>-<strong>Color</strong> Imprägnier-<strong>Lasur</strong> <strong>TC</strong> <strong>6303</strong> farbig (coloured) and one coat<br />

of Imprägnier-<strong>Lasur</strong> farblos (colourless).<br />

Note: Colourless <strong>Tex</strong>-<strong>Color</strong> Imprägnier-<strong>Lasur</strong> <strong>TC</strong> <strong>6303</strong> can be used<br />

to lighten darker colours. Do not use the colourless product on its<br />

own.<br />

Quantities<br />

Cleaning of tools<br />

Drying time<br />

Application temperature<br />

Approx. 12 ml/m², dependent on the roughness of the substrate.<br />

If a precise calculation is required then a test coat should be applied<br />

to an appropriate surface.<br />

Clean using turpentine substitute or <strong>Tex</strong>-<strong>Color</strong> Pinselreiniger paint<br />

brush cleaner.<br />

Dust dry after approx. 4 hours at temperatures of approx.+20 °C and<br />

max. 65% humidity. Touch dry after approx. 8 hour. Can be sanded<br />

and painted over after approx. 12 hours.<br />

These times may increase depending on the temperature and<br />

humidity.<br />

The temperature of the surrounding environment and item being<br />

painted should be at least +5 °C during application and drying.<br />