Images taken after the firing with alumina. Images taken by Dave- the

warping has been stopped- successful way of stopping warping in the kiln.

Making plaster bats of the same width, to stop the walls from being different

thicknesses. I sand blasted a sheet of glass to sand the plaster on as the metal

cottles are slightly bowed, causing the plaster bats to have a slight curve. I could

make my own cottles out of plastic or a coated wood to eliminate the need for

this stage as it is time consuming and not as accurate as it could be.

Resolutions for cracking and warping:

-Grog and slip ratio

-Use of alumina in the kiln

To Do: Use a softer support to stop warpage when drying, one that won’t

cause cracks when drying