<strong>PRESENTATIE</strong><br />

PRE - ANODISEREN<br />

<strong>ALUMINIUM</strong> CENTRUM <strong>NL</strong><br />

Dirk Boonen Alural Group <strong>29</strong>.<strong>09</strong>.<strong>2010</strong>


Pré - Anodiseren<br />

DEEL I<br />

Voorstelling van de Alural Group<br />

DEEL II<br />

PRE-ANODISEREN ALS VOORBEHANDELING


DEEL I :<br />

VOORSTELLING<br />

ALURAL GROUP<br />

De historiek<br />

De activiteiten<br />

De klanten


HISTORIEK<br />

<br />

<br />

<br />

<br />

Gesticht in 1986 met 1 kleine fabriek in Boom door<br />

André de Rooy en Georges de Colfmaeker.<br />

Evolutie naar oppervlaktebehandelen &<br />

dienstenverlenen<br />

logistiek diensten<br />

verkoop aanverwante producten<br />

Sinds 2001 onderdeel van beursgenoteerde group<br />

Ackermans & van Haaren .<br />

Belangrijkste onafhankelijke looncoater in Europa:<br />

350 werknemers<br />

€ 37,4 mio omzet<br />

2 plants in België, 1 in Frankrijk en 1 in Polen


ACTIVITEITEN<br />

Oppervlaktebehandeling<br />

Poedercoaten<br />

Pre-Anodiseren<br />

Anodiseren van<br />

stukwerk<br />

Natlakken on site<br />

Houtdecoratie<br />

Diverse diensten<br />

Handelsplaten<br />

Knip- en Zetwerk<br />

Sandwich panelen<br />

Montage beslag<br />

Warehousing<br />

Thermisch isoleren


ALURAL Lummen


Pre-Anodiseren


Poedercoaten


Poedercoaten


Houtdecoratie


Thermisch isoleren


KLANTEN<br />

De Alural Group is een van de grootste<br />

onafhankelijke looncoaters in Europa en<br />

verzorgt het poedercoatwerk en andere<br />

diensten voor :<br />

- Extruders<br />

- Systeemhuizen<br />

- Groothandels<br />

- Fabrikanten<br />

- constructeurs


DEEL I I :<br />

PRE ANODISEREN<br />

Voorbehandelingen bij de ALURAL GROUP<br />

Waarom Pré-anodiseren<br />

PRE ANODISEREN<br />

Het proces<br />

Eigenschappen<br />

Zeer hoge weerstand tegen Filiforme corrosie<br />

Mechanisme


VOORBEHANDELINGEN<br />

<br />

<br />

<br />

<br />

<br />

Alural France : Dompelen chromateren<br />

Alural Poland: : Sproeistraat chromateren<br />

Alural Belgium (Tisselt): Chromateren sproeien<br />

2 lijnen horizontaal ; 1 lijn vertikaal met cascade<br />

1 dompelstraat voor gietstukken<br />

Alural Lummen : Chromateren sproeien horizontaal<br />

+ vertikaal<br />

Pré-anodiseren<br />

te Lummen t.b.v. alle laklijnen<br />

<strong>2010</strong>: Nieuwe horizontale : testfase Zirkoniseren spr.<br />

2011: Nieuwe Vertikale (2011) : ?


Waarom pré-anodiseren<br />

<br />

<br />

<br />

<br />

<br />

<br />

Onderzoek substraat: Nordlien, Defrancq, Züst, Benmalek,<br />

Stuckart: Warmtebehandeling alu veroorzaakt een actieve<br />

toplaag : >2 g/m²<br />

beitsen. ? Niet steeds voldoende<br />

Pietschmann, Gardein, FEM (D): FFC & Results of 10 years<br />

natural weathering: enkel préano binnen de FFC - norm<br />

Qualisino: Technologisch artikel adviseert préano<br />

Standpunt en ervaringen van nog vele andere grote spelers op<br />

de markt, zoals Schüco, Permasteelisa, etc<br />

Een chroomvrije voorbehandeling met de beste<br />

corrosiewering voor agressieve klimaten<br />

Eigen ervaringen gedurende jaren aan de Belgische kust


Abstract<br />

The filiform corrosion susceptibility of extruded, chromated and coated AA 6060/6063<br />

alloys has been investigated. It is shown that, provided sufficient metal is removed<br />

before chromating, these alloys will exhibit high filiform corrosion resistance. In those<br />

cases where extensive filiform corrosion attack is observed during corrosion testing it is<br />

shown to be due to a reactive surface region, formed during the thermo-mechanical<br />

processing of the alloy and remaining after chemical pretreatment for painting.<br />

Das Auftreten von Filiformkorrosion auf lackierten Aluminiumprofilen<br />

Die Anfälligkeit chromatierter und lackierter Strangpressprofile aus den Legierungen AA<br />

6060/6063 für Filiformkorrosion ist untersucht worden. Es wird gezeigt, dass bei einem<br />

genügenden Metallabtrag vor dem Chromatieren diese Legierungen eine hohe<br />

Beständigkeit gegenüber Filiformkorrosion aufweisen. In den Fällen, bei welchen<br />

während der Korrosionsprüfungen ein ausgedehnter Angriff durch Filiformkorrosion<br />

auftritt, wird nachgewiesen, dass dies an empfindlichen Oberflächenregionen<br />

geschieht, die während der thermo-mechanischen Verarbeitung der Legierungen<br />

entstanden sind und in der chemischen Vorbehandlung nicht entfernt wurden.<br />

Get PDF (178K)<br />

More content like this<br />

Find more content: like this article<br />

Find more content written by: J. H. Nordlien<br />

J. Defrancq<br />

W. Züst<br />

M. Benmalek<br />

R. Stuckart<br />

All Authors


FFC & Results of 10 years<br />

natural weathering


FFC & Results of 10 years<br />

natural weathering


FFC & Results of 10 years<br />

natural weathering


FFC & Results of 10 years<br />

natural weathering


FFC & Results of 10 years<br />

natural weathering


FFC & Results of 10 years<br />

natural weathering


FFC & Results of 10 years<br />

natural weathering


FFC & Results of 10 years<br />

natural weathering


FFC & Results of 10 years<br />

natural weatering


Diverse processen:<br />

<br />

PRE-ANODISEER<br />

PROCES<br />

Chroomzuur : luchtvaartindustrie: verlijmen<br />

Fosforzuur : AC / DC 60°C<br />

Zwavelzuur : DC 25-30°C meest gebruikt als<br />

voorbehandeling in architectuur<br />

toepassingen


PRE-ANODISEER<br />

PROCES bij Alural<br />

Licht alkalisch ontvetten / Spoelen<br />

Alkalisch beitsen / Spoelen<br />

Neutraliseren / Spoelen<br />

Anodiseren 5 – 8 µm H2SO<br />

SO4 : 190 g/l<br />

Al < 15 g/l A/dm² dm²: 1,5 T: 27°C<br />

Demi-spoelen<br />

Demi-spoelen<br />

Demi-spoelen<br />

Droogspoelen in demiwater van 60°C


PRE-ANODISEER<br />

PROCES bij Alural<br />

BELANGRIJKE PARAMETERS<br />

• Goede voorbehandeling (beits)<br />

• Verhoogde Temperatuur : grotere poriën<br />

• Laagdikte van 6 à 7 µ beste corrosiewering<br />

• Spoeling : fosfaatresten onthechting


EIGENSCHAPPEN<br />

Zeer dikke conversielaag 5 – 8 µ t.o.v.<br />

chroom : 0,25 – 0,5 µ /Zirkoon: 0,05 – 0,1 µ<br />

2/3 van de dikte is volume van substraat en<br />

1/3 extra volume: actieve toplaag met<br />

precipitaten van vreemde elementen is weg<br />

Miljarden poriën/cm² cm²: porositeit = hechting<br />

Elektrische weerstand (barrier<br />

layer)<br />

verhindert vorming van galvanische cel<br />

Zeer efficiënt in het verhinderen van FFC


FFC MECHANISME<br />

Initiatie door bv Cl- kan op het oppervlak via<br />

een zwakke plaats in de coating(niet door de<br />

préanodiseerlaag), maar meestal via niet<br />

beschermde beschadigingen(zagen, boren):<br />

aantasting van een vreemd element.<br />

<br />

coating<br />

Cr<br />

Fig. 1 : aantasting ergens op de zaagsnede : oplossen van metaal; vorming van hydroxide<br />

tot oxide. Kop wordt zuur H+ en lost het Al verder op, met vorming van<br />

oxideprodukten die via de staart geen zuurstof meer toelaten en de laklaag omhoog<br />

duwen .<br />

Actieve laag<br />

Al


FFC MECHANISME


FFC MECHANISME<br />

FFC= draadvormige corrosie onder het grensvlak met de<br />

conversielaag of coating, die voortkruipt in de wals- of<br />

extrusierichting door de hoge zuurtegraad in de kop.<br />

Draden kruisen elkaar niet en als ze elkaar ontmoeten<br />

stopt het proces door de reactie van de zure kop met<br />

het in de andere draad gevormde Al2O3, waardoor de<br />

zuurtegraad wordt gereduceerd en geneutraliseerd.<br />

Dit is precies wat er gebeurt als de zure kop in aanraking<br />

komt met het Al2O3 van de préanolaag, waardoor de<br />

zuurtegraad daalt en de oplosreactie stopt.


REFERENTIEPROJECTEN<br />

Blitta<br />

Van Dool<br />

Oskomera<br />

: Le Maire Arnhem<br />

: Spoorzone Berkel en Rodenijs<br />

Gemeentehuis Lansingerland<br />

: ENECO Rotterdam<br />

Vorsselmans : Broekman Rotterdam<br />

Auxilla<br />

Sculptura Breda<br />

ROC Mondriaan<br />

ROC Brasserskade


REFERENTIEPROJECTEN<br />

SAPA BUILDING Systems: Rollecate<br />

REYNAERS <strong>ALUMINIUM</strong>:<br />

Oskomera : Wassenaarseweg Leiden<br />

Hermeta<br />

: Merwedehoofd Papendrecht<br />

Groothandelsgebouw Rotterdam<br />

Paradijslaan<br />

van Hoesel: Betonsingel Wateringen


PRE - ANODISEREN<br />

DE ENIGE VOORBEHANDELING MET EEN<br />

VERZEKERDE GARANTIE TEGEN HET<br />

OPTREDEN VAN FILIFORME CORROSIE<br />

OOK BIJ ZAAGSNEDEN EN PONSGATEN


PRE - ANODISEREN<br />

Met dank voor uw aandacht<br />

pleit Alural voor een duurzame<br />

oppervlaktebehandeling van de<br />

elementen van uw steeds<br />

duurzamer en functioneler<br />

wordende aluminium gevels

Hooray! Your file is uploaded and ready to be published.

Saved successfully!

Ooh no, something went wrong!