Lap shear strength versus temperature (ISO 4587) (typical average values)Cure: (a) = 7 days /23 C; (b) = 24 hours/23 C + 30 minutes/80 CMPa30252015ba105°C0-60 -40 -20 0 20 40 60 80 100Roller peel test (ISO 4578)Cure: 16 hours /40 o C4.0 N/mmTensile strength at 23 C (ISO 527)Tensile modulusElongation at break7 MPa16 MPa45 %Lap shear strength versus immersion in various media (typical average values)Unless otherwise stated, L.S.S. was determined after immersion for 90 days at 23 C30 days 60 days 90 daysCure: 16 hour/40°CAs-made valueIMSD egradedGasoline (petrol)Ethyl acetateAcetic acid, 10%D egradedXyleneLubricating oilParaffinWater at 23°CWater at 60°CWater at 90°CMPa0 2 4 6 8 10March 2009 <strong>Araldite</strong> ® <strong>AY</strong> <strong>4446</strong> / <strong>Hardener</strong> <strong>HY</strong> <strong>4445</strong> Page 4 of 6

Hooray! Your file is uploaded and ready to be published.

Saved successfully!

Ooh no, something went wrong!