- Page 1 and 2: Corrosion Control for Water &Wastew
- Page 3 and 4: Corrosion
- Page 5 and 6: Corrosion Cell on Buried PipingCath
- Page 10 and 11: History of Iron PipeCast Iron- Intr
- Page 12 and 13: 1.58 in.1.22 in.0.94 in.0.87 in.0.5
- Page 14 and 15: Adverse Conditions for Metallic Pip
- Page 16 and 17: Coupling to Dissimilar MetalsMetall
- Page 18 and 19: Anode Installation Prevents Corrosi
- Page 20 and 21: Meter Vaults(Keep dry if possible)
- Page 22 and 23: Dissimilar Surface ConditionsPipe(C
- Page 24 and 25: Gas Pipeline(-)Cathodic ProtectionR
- Page 26 and 27: PowerStationStray Current by DCOper
- Page 28 and 29: Bonding Across a Bell and Spigotor
- Page 30 and 31: Potentials (millivolts)00+0500+1000
- Page 32 and 33: Polyethylene Encasement of Ductile
- Page 34 and 35: PRACTICAL GALVANIC SERIESMaterialPo
- Page 36 and 37: Galvanic AnodeStructureMagnesiumAno
- Page 38 and 39: Anode InstallationAugered holeGalva
- Page 40 and 41: Number of Breaks25100 Breaks Prior
- Page 42 and 43: Repair of Break ShouldInclude Anode
- Page 44 and 45: Lower Stress Area(Cathode)PipeThrea
- Page 46 and 47: Anode Installed on Metallic Fitting
- Page 48 and 49: Bolt Corrosion(due to water/sludge)
- Page 50 and 51: Suspended Horizontal Anode SystemTo
- Page 52 and 53: Annual Maintenance
- Page 54 and 55: Pumping StationsCORRPROC O M P A N
- Page 57 and 58:
AC Mitigation
- Page 59 and 60:
Insituform
- Page 61 and 62:
QUESTIONS ?James T LaryCorrpro Comp
- Page 63 and 64:
Cathodic Protection of Metallic Fit
- Page 65 and 66:
Corrosion of Metallic Structure
- Page 67 and 68:
SummaryReducing corrosion rates on
- Page 70 and 71:
AbovegroundStorage TankTest/AccessS
- Page 72 and 73:
Budget Estimate for CompleteCathodi
- Page 74 and 75:
Corrosion Protection DesignPhase II
- Page 76 and 77:
Transformer Rectifier
- Page 78:
Yard Piping Deep Anode GroundbedImp
- Page 81 and 82:
Bi-Metallic Corrosion BetweenCarbon
- Page 83 and 84:
Repair of Break ShouldInclude Anode
- Page 85:
Corrosion Control for Water& Wastew
- Page 88 and 89:
Bolt & Nut Corrosion
- Page 90 and 91:
Basic Corrosion CellGround SurfaceB
- Page 92:
Corrosion Can be Defined as Either:
- Page 97 and 98:
Dissimilar SoilsPavementSandy LoamC
- Page 99 and 100:
Proper Handling & Installation ofPo
- Page 101 and 102:
Corrosion Pitting
- Page 103:
Corrosion Caused by DifferentialAer
- Page 106 and 107:
Number of Breaks2094 Breaks Prior t
- Page 108 and 109:
Number of Breaks2094 Breaks Prior t
- Page 110 and 111:
Corrosion on damaged polyethylene e
- Page 112 and 113:
Cathodic Protection Test StationTes
- Page 115 and 116:
Cathodic Protection for Hot Water T
- Page 117 and 118:
PCCP Failure
- Page 119 and 120:
Pre-stressed Concrete Cylinder Pipe
- Page 121 and 122:
Corrosion Control & Cathodic Protec
- Page 123:
Corrosion Can be Defined as Either: