Australian’s Molten Salt Reactor (MSR) Material Research Ondrej Muránsky
11_Ondrej_Muransky
11_Ondrej_Muransky
You also want an ePaper? Increase the reach of your titles
YUMPU automatically turns print PDFs into web optimized ePapers that Google loves.
ANSTO Corrosion Testing<br />
• ANSTO-SINAP JRC (<strong>MSR</strong>)<br />
– FLiNaK salt composition<br />
– Tests conducted at 650ºC - 750ºC for<br />
10, 100 and 200 h<br />
• SINAP <strong>Material</strong>s<br />
– GR 3535, Graphite, NiMo-SiC,<br />
Hastelloy-N<br />
Hastelloy-N, Electron Back-Scatter Diffraction (EBSD) and<br />
Energy Dispersive Spectroscopy (EDS) chromium (Cr)<br />
distribution map, 200h/650C, FLiNaK.