liant<br />

T début = 5°C<br />

LE BITUME : essai bille et anneau<br />

Norme EN 1427<br />

bille<br />

anneau<br />

T bille et anneau<br />

avant après<br />

Chauffage + agitation<br />

(+ 5°C/min)<br />

Classes 20/30 35/50 50/70 70/100 160/220<br />

TBA (°C) 55/63 50/58 46/54 43/51 35/43<br />

Les <strong><strong>en</strong>robés</strong> bitumineux : formulation, fabrication, mise <strong>en</strong> place – Montréal 2006<br />

41