STANDARDISED CRUSHING TESTS<br />

Crushing strength of a PVC tube<br />

Crushing strength of a ductile cast iron pipe<br />

Due to the rigidity of ductile cast iron, the PAM<br />

pipeline system resists deformities and retains<br />

its linearity, ensuring respect of the water flow.<br />

What seems like a mechanical paradox should be<br />

considered with interest, since it is the combination<br />

of these characteristics which gives the PAM pipeline<br />

system its longevity, ensuring it remains watertight<br />

over time, in spite of contingencies.<br />

DN<br />

Rigidity<br />

kN/m 2<br />

Ovalisation<br />

%<br />

150 230 1,9<br />

200 105 2,5<br />

250 66 2,8<br />

300 47 3,0<br />

400 31 3,2<br />

500 22 3,4<br />

800 20 4,0<br />

1000 16 4,0<br />

DIAMETRICAL RIGIDITY OF THE TAG 32® RANGE<br />

Corresponds to 32 kN/m2 and meets the need for<br />

performance in the gravity market perfectly.<br />

DN<br />

Rigidity<br />

kN/m 2<br />

Ovalisation<br />

%<br />

150 74 1,5<br />

300 32 3,0<br />

Saint-Gobain PAM - SEWERAGE - 2012<br />

17