Comparative Shear Bond Strength to<br />
Dentin<br />
OptiBond <strong>XTR</strong> Comparative Dentin Bond Strengths vs. Leading Adhesives<br />
OptiBond <strong>XTR</strong><br />
ClearFil SE<br />
Xeno® IV<br />
iBond®<br />
OptiBond FL<br />
0 5 10 15 20 25 30 35 40 45<br />
Shear Bond Strength (MPa)<br />
• OptiBond <strong>XTR</strong> demonstrated comparable<br />
dentin bond strengths to Xeno IV<br />
• OptiBond <strong>XTR</strong> demonstrated higher<br />
dentin bond strengths than total-etch<br />
and other self-etch adhesives<br />
Data on File<br />
Kerr Corporation