Shear Bond Strength (MPa)<br />
OptiBond <strong>XTR</strong> was NOT light cured. Cements were allowed to self-cure<br />
Comparative Indirect Dentin Shear Bond Strength<br />
Using Self-Cured Resin Cements (No light Curing of<br />
<strong>XTR</strong>)<br />
OptiBond <strong>XTR</strong> Comparative Indirect Dentin Bond Strengths with Resin Cements<br />
22<br />
20<br />
18<br />
16<br />
14<br />
12<br />
10<br />
8<br />
6<br />
4<br />
2<br />
0<br />
18.7<br />
19.3<br />
OptiBond <strong>XTR</strong> + NX3 MultiLink Primer A & B +<br />
MultiLink Cement<br />
11.2<br />
ED Primer AB/Panavia F2.0<br />
Cement<br />
• The combination of OptiBond<br />
<strong>XTR</strong> + NX3 cement<br />
demonstrated comparable<br />
indirect dentin bond strength to<br />
the Multilink Cementation<br />
System<br />
• OptiBond <strong>XTR</strong> showed much<br />
higher indirect dentin bond<br />
strength vs. the Panavia<br />
Cementation System<br />
Data on File,<br />
Kerr Corporation