UW-52 (c)<br />

Degree of RT<br />

Unacceptable imperfections<br />

Spot<br />

1. indication characterized as a crack or zone of incomplete fusion or<br />

penetration.<br />

2. Welds having indications characterized as slag inclusions or cavities<br />

are unacceptable when;<br />

a. the indication length exceeds 2/3 t, where t is defined as shown in<br />

UW-51(b)(2).<br />

b. For all thicknesses, indications less than ¼ in. (6 mm) are acceptable,<br />

and indications greater than ¾ in. (19 mm) are unacceptable.<br />

c. Multiple aligned indications meeting these acceptance criteria are<br />

acceptable when the sum of their longest dimensions indications does<br />

not exceed t within a length of 6t (or proportionally for radiographs<br />

shorter than 6t), and when the longest length L for each indication is<br />

separated by a distance not less than 3L from adjacent indications.<br />

(3) Rounded indications are not a factor in the acceptability of welds not<br />

required to be fully radiographed.<br />