CUT BACK TECHNIQUE – FINISHING<br />

10<br />

Cut off the sprues carefully using a suitable cut-off-disc. Work<br />

with low <strong>press</strong>ure and low r.p.m. (revolutions per minute). After<br />

separating, the work is carefully fitted onto the die.<br />

Caution in the area <strong>zirconium</strong> <strong>oxide</strong>/<strong>press</strong> ceramic: Intense heat<br />

can ca<strong>use</strong> breaks!<br />

The fully anatomically modelled restoration should be reduced<br />

or prepare the already reduced restoration <strong>for</strong> veneering.