16<br />

Fig. 16. Inside surface <strong>of</strong> standard Hastelloy N tubing, exposed <strong>to</strong> salt at 620-640°C. Location E, Fig. 11. (a) As<br />

polished, (b) etched with glyceria regia. SOOX.<br />

Fig. 17. Inside surface <strong>of</strong> standard Hastelloy N tubing, exposed <strong>to</strong> salt at 604-620°C. Location F, Fig. 11. (a) AS<br />

polished, (b) etched with glyceria regia. SOOX.