c) 50% coarse pearlite + 25% bainite + 25% martensite: To do this, we will<br />

need to have a three step process. First, cool to a temperature above the<br />

nose of the IT curve and hold until you have converted 50% of the austenite<br />

to coarse pearlite. Second, rapidly cool to a temperature below the nose, but<br />

above the M start temperature, and hold until 50% of the remaining austenite is<br />

converted to bainite (this makes 50% of 50% = 25% bainite). Finally, rapidly<br />

quench through the Mf temperature to completely convert the remaining<br />

austenite to martensite