<strong>DSC</strong>: Oxidative Stability (OIT) Method<br />
OIT Method<br />
1) Equilibrate at 60°C<br />
2) Isothermal for 5.00 min.<br />
3) Ramp 20°C/min. to 200°C<br />
4) Isothermal for 5.00 min.<br />
5) Abort next seg. if W/g > 1.0<br />
6) Select gas: 2<br />
7) Iso-track for 200.00 min.<br />
<strong>DSC</strong>: Modulated <strong>DSC</strong> Method<br />
M<strong>DSC</strong> Method<br />
1) Data storage: off<br />
2) Equilibrate at -20°C<br />
3) Modulate ±1°C every 60 seconds<br />
4) Isothermal for 5.00 min.<br />
5) Data storage: on<br />
6) Ramp 3°C/min. to 300°C