<strong>DSC</strong>: Cell Schematic Diagram<br />
Chromel<br />
Disc<br />
Dynamic Sample Chamber<br />
Reference Pan<br />
Gas Purge Inlet<br />
Heating<br />
Block<br />
Alumel Wire<br />
Chromel Wire<br />
<strong>DSC</strong>: Cell Components<br />
Sample Pan<br />
Lid<br />
Chromel<br />
Disc<br />
Thermocouple<br />
Junction<br />
Thermoelectric Disc<br />
(Constantan)<br />
Silver Furnace: for good temperature<br />
uniformity<br />
Sample Purge: for excellent oxidative<br />
stability measurements<br />
Purge Preheated: for very low noise from<br />
turbulence<br />
Air Cool: for fast return to room<br />
temperature