Differential Scanning Calorimetry (DSC)
Differential Scanning Calorimetry (DSC)
Differential Scanning Calorimetry (DSC)
You also want an ePaper? Increase the reach of your titles
YUMPU automatically turns print PDFs into web optimized ePapers that Google loves.
<strong>DSC</strong>: Effect of Heating Rate<br />
on Indium Melting Temperature<br />
Heat Rate Onset Peak ∆H<br />
Onset<br />
Variation<br />
to 10°C/min<br />
2°C/min 156.49°C 156.61°C 28.46 J/g -0.12°C<br />
5 156.54 156.75 28.45 -0.07<br />
10 156.61 156.87 28.46 0<br />
20 156.76 157.08 28.44 +0.15<br />
<strong>DSC</strong>: Polymer Sample w/Internal<br />
Temperature Calibration Material<br />
2 Layers<br />
of Polymer<br />
Film<br />
Melting Point<br />
Standard, e.g.<br />
Indium<br />
Typical weight of polymer sample is 10mg<br />
(2 films at 5mg each) with 1-3mg of Indium