GETCO/E/TS – XMER01power/R4 Sept <strong>08</strong><br />

Sr. Characteristics of Transformer Requirement<br />

Method of test<br />

No.<br />

Oil<br />

13 Ageing Characteristics after 96<br />

Hrs accelerated ageing (Open<br />

ASTM-/D<br />

1934/IS: 12177<br />

beaker method with copper<br />

catalyst)<br />

a) Specific Resistance<br />

(Resistivity)<br />

1) @ 27 0 C<br />

2) @ 90 0 C<br />

b) Dielectric Dissipati<strong>on</strong> Factor<br />

2.5 X 10 12 Ohm-cm-Min.<br />

0.2 X 10 12 Ohm-cm min.<br />

0.2 Max.<br />

(Tan delta) @ 90 0 C<br />

c) Total acidity<br />

d) Total sludge value<br />

0.05 mg. KOH/gm Max.<br />

0.05 % by weight Max.<br />

14 Presence of Oxidati<strong>on</strong> inhibiti<strong>on</strong> Absent IS: 335<br />

Appendix: D<br />

15 Water c<strong>on</strong>tent PPM (Max)<br />

New untreated oil<br />

After treatment<br />

50 PPM Max.<br />

05 PPM Max.<br />

IS: 2362<br />

IS: 18<str<strong>on</strong>g>66</str<strong>on</strong>g><br />

16 Poly Chlorinated Biphenyls NIL IEC 61619<br />

(PCB) C<strong>on</strong>tent<br />

Doble spec<br />

17 Gassing tendency at 50 hZ, after<br />

120 minutes<br />

5 mm 3 per minute (Max.) Doble spec<br />

SEAL OF COMPANY<br />

DATE:<br />

SIGNATURE OF BIDDER<br />

Sign and Seal of Bidder Page 63 of 87

Hooray! Your file is uploaded and ready to be published.

Saved successfully!

Ooh no, something went wrong!