Figure 2. 50 µ<strong>in</strong> thick gold plated<br />

conductor pads after 500 hrs at 125<br />

ºC. This is typical of appearance of<br />

similar conductor pads.<br />

Figure 3. 50 µ<strong>in</strong> thick gold plated<br />

conductor pads after 1,000 hrs at<br />

125 ºC. Note good uniform<br />

appearance.<br />

Figure 4. 20 µ<strong>in</strong> thick electroless gold<br />

plated conductor pads after 1,000 hrs at<br />

125 ºC. Note blister<strong>in</strong>g.<br />

Slide 12