Record axial deformation, shear deformation, axial load, and shear load during<br />

intervals shown in table 4 or at other appropriate intervals.<br />

7.--The test takes about 70 to 80 minutes to complete from the time the specimen is placed in the<br />

removed.<br />

Suggested Data Collection for the Repeated Shear Test at a Field State of Stress<br />

Collected During Cycles:<br />

1 through 10 1,747 through 1,750<br />

20 through 22 2,000 through 2,002<br />

30 through 32 2,247 through 2,250<br />

50 through 52 2,500 through 2,502<br />

80 through 82 2,748 through 2,750<br />

100 through 102 2,997 through 3,000<br />

200 through 202 3,200 through 3,202<br />

300 through 302 3,400 through 3,402<br />

400 through 402 3,600 through 3,602<br />

500 through 502 3,800 through 3,802<br />

600 through 602 3,997 through 4,000<br />

800 through 802 4,200 through 4,202<br />

1,000 through 1,002 4,500 through 4,502<br />

1,247 through 1,250 4,998 through 5,000<br />

1,500 through 1,502<br />

duration of each cycle is 0.7 second.<br />

collection rate of 60 data points per second is satisfactory.<br />

Volumetric Test<br />

Place the specimen (prepared in accordance with sections 6.1 and 6.2) between<br />

bottom platens.<br />

Surround the specimen with a membrane,<br />

open at both ends and free of any defects.<br />

150 mm in diameter and 0.6 mm<br />

Fix the membrane tightly to the platens with rubber O-rings.<br />

Mount a radial LVDT around the circumference of the specimen to measure its<br />

deformation. Then mount LVDTs on both sides of the specimen to measure axial<br />

from platen to platen.<br />