Q24. During inspection of a parallel sided machined <strong>for</strong>ging using straight<br />

beam immersion techniques, a diminishing back reflection in a localized<br />

area in the absence of a defect indication would least likely represent:<br />

A. A course grain structures<br />

B. A small non-metallic stringer<br />

C. A defect oriented at a severe angle to the entry surface<br />

D. A large inclusion.